MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zircar Refractory Composites RS-A Refractory Sheet
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ZRCI`s Refractory Sheet Type RS-A Moldable is a tough ceramic fiber reinforced insulation which contains no asbestos. Developed as an asbestos board replacement for induction coil liners and molten metal transport, Refractory Sheet Type RS-A Moldable is ideally suited for a wide range of high temperature, high thermal shock applications. Refractory Sheet Type RS-A Moldable is a wet blanket that can be easily formed into a wide variety of simple and complex shapes. Drying results in a strong rigid shape that can be rewet to restore the original moldability. Baking irreversibly removes the moldability, leaving Refractory Sheet Type RS-A Moldable unaffected by moisture. Refractory Sheet Type RS-A Moldable can be frozen and thawed repeatedly with no loss in moldability or other properties. Refractory Sheet Type RS-A Moldable can be dried rapidly, either with a torch or by applying directly to a hot furnace, to make quick repairs of cracks in, or to replace missing, refractories.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 - 1.70 g/cc
Solids Content 65 %
Porosity 40 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00345 GPa
 0.00550 GPa
@Temperature 1000 °C,
Time 57600 sec
Compressive Yield Strength 69.0 MPa10% compression
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.047 J/g-°C
Thermal Conductivity 0.650 W/m-Kperpendicular to thickness
Maximum Service Temperature, Air 1450 °C
Shrinkage <= 1.0 %drying, perpendicular to thickness
 16 - 20 %drying, parallel to thickness
 4.0 %
@Temperature 1200 °C,
Time 57600 sec
linear perpendicular to thickness
 
Component Elements PropertiesOriginal ValueComments
Al2O3 90 - 92 %
SiO2 6.0 - 10 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Refractory Composites RS-99-45 Refractory Sheet
Zircar Refractory Composites RS-A3 Refractory Sheet
Zircar Refractory Composites RS-99-60 Refractory Sheet
DWA 6091/SiC/20p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)
Zircar Refractory Composites RS-A1 Refractory Sheet

CZRCI29 / 2892

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.