MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® B 4300 G6 High Speed Unc. 30% Glass Filled PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Ultradur B 4300 G6 High Speed Unc. is a high flow, fast cycling with low warpage, 30% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable applications.

Applications: Housings, consoles, contact carriers, and covers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³ISO 1183
Water Absorption 0.40 %0.40 %DIN 53495/1L
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C/50% R.H.
Viscosity Number 87 cm³/g0.87 dl/gISO 1628
Linear Mold Shrinkage, Flow 0.0036 cm/cm0.0036 in/in60x60x2mm; ISO 294
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/in60x60x2mm; ISO 294
Melt Flow 33.7 g/10 min
@Load 2.16 kg,
Temperature 250 °C
33.7 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 135 MPa19600 psi50mm/min; ISO 527-2
Elongation at Break 2.6 %2.6 %50mm/min; ISO 527
Modulus of Elasticity 9.70 GPa1410 ksiISO 527-2
Charpy Impact Unnotched 50.0 J/cm²238 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 7.50 J/cm²35.7 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 350 V350 VTest Solution A; IEC 112
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 - 225 °C428 - 437 °F
Maximum Service Temperature, Air 210 °C410 °F
Deflection Temperature at 0.46 MPa (66 psi) 221 °C430 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 202 °C396 °FISO 75-2
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 275 °C482 - 527 °FInjection molding
Mold Temperature 60.0 - 100 °C140 - 212 °F
 
Descriptive Properties
ColorNatural and Black
Commercial StatusNorth America and Europe
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® B 4300 G6 30% Glass Filled PBT
BASF Ultradur® B 2550 PBT
BASF Ultradur® B 4500 PBT
BASF Ultradur® B 4300 G2 10% Glass Filled PBT
BASF Ultradur® B 4040 G6 LS High Speed BK15029 30% Glass Filled PBT/PET

PBASF9078 / 84842

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.