MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 5457-O
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A95457; Aluminium 5457-O; AA5457-O; Al5457-O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.69 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 32AA; Typical; 500 g load; 10 mm ball
Tensile Strength, Ultimate 19.0 ksiAA; Typical
Tensile Strength, Yield 7.00 ksiAA; Typical
Elongation at Break 22 %
@Thickness 1.59 mm
AA; Typical
Modulus of Elasticity 10000 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Poissons Ratio 0.33
Shear Modulus 26.0 GPaCalculated
Shear Strength 12.0 ksiAA; Typical
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 23.0 ohm-cir-mil/ft
@Temperature 20.0 °C
AA; Typical
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.2 µin/in-°F
@Temperature 20.0 - 100 °C
AA; Typical; average over range
 21.9 µm/m-°C
@Temperature -50.0 - 20.0 °C
 23.7 µm/m-°C
@Temperature 20.0 - 100 °C
 24.6 µm/m-°C
@Temperature 20.0 - 200 °C
 25.6 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.880 J/g-°CEstimated from trends in similar Al alloys.
Thermal Conductivity 1220 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 1165 - 1210 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 1165 °FAA; Typical
Liquidus 1210 °FAA; Typical
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 650 °Fholding at temperature not required
Hot-Working Temperature 500 - 950 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 97.7 %As remainder
Copper, Cu <= 0.20 %
Iron, Fe <= 0.10 %
Magnesium, Mg 0.80 - 1.2 %
Manganese, Mn 0.15 - 0.45 %
Other, each <= 0.03 %
Other, total <= 0.10 %
Silicon, Si <= 0.08 %
Vanadium, V <= 0.05 %
Zinc, Zn <= 0.05 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 5657-O
Aluminum 5456-O
Aluminum 5454-O
5049 Aluminum Composition Spec
Aluminum 5005-H14

MA5457O / 9291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.