MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BASF Ultramid® A 246M Natural Nylon 66, Impact Modified, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Product Description: Ultramid® A 246M Natural is an unfilled polyamide 6.6, impact modified, for injection molding. This grade offers an excellent impact resistance, even at a low temperature.

Availability: Africa & Middle East; Asia Pacific; Latin America; North America

Additive: Impact Modifier

Features: Good Mold Release; High Impact Resistance; Low Temperature Impact Resistance

Use: Automotive Applications; Consumer Applications; Footwear; Outdoor Applications; Power/Other Tools; Sporting Goods

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Appearance: Black; Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA66

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Water Absorption 1.1 %
@Time 86400 sec
1.1 %
@Time 24.0 hour
ISO 62
Maximum Moisture Content 0.200.20
Linear Mold Shrinkage, Flow 0.016 cm/cm0.016 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 44.0 MPa6380 psiISO 527-2
Tensile Strength, Yield 43.6 MPa6320 psiISO 527-2
 50.0 MPa7250 psiASTM D638
Elongation at Break 80 %80 %ASTM D638
Elongation at Yield 20 %20 %ISO 527-2/50
Tensile Modulus 1.90 GPa276 ksiISO 527-1
Flexural Strength 70.3 MPa10200 psiISO 178
 70.3 MPa10200 psiASTM D790
Flexural Modulus 1.80 GPa261 ksiISO 178
 1.80 GPa261 ksiASTM D790
Izod Impact, Notched 1.01 J/cm1.90 ft-lb/inASTM D256
Izod Impact, Notched (ISO)  21.0 kJ/m²
@Temperature -30.0 °C
10.0 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 60.9 kJ/m²
@Temperature 22.8 °C
29.0 ft-lb/in²
@Temperature 73.0 °F
ISO 180/A
Charpy Impact Unnotched  1.60 J/cm²
@Temperature -30.0 °C
7.60 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
ISO 179/1eU
Charpy Impact, Notched 9.66 J/cm²46.0 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 62631-3-1
Dielectric Constant 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 62631-2-1
Dielectric Strength  22.0 kV/mm
@Thickness 2.00 mm
560 kV/in
@Thickness 0.0787 in
IEC 60243-1
 35.0 kV/mm
@Thickness 0.800 mm
890 kV/in
@Thickness 0.0315 in
IEC 60243-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 450 V450 VSolution B; IEC 60112
 575 V575 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C145 °FUnannealed; ASTM D648
 65.0 °C149 °FUnannealed; ISO 75-2/A
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
IEC 60695-11-10,-20
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 265 - 275 °C509 - 527 °F
Middle Barrel Temperature 270 - 280 °C518 - 536 °F
Front Barrel Temperature 280 - 285 °C536 - 545 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2078 / 310771

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.