MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Celanese Celstran® PPS-GF40-01 PPS, 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: 40% long strand fiber glass reinforced polyphenylene sulfide
40% long strand fiber glass reinforced polyphenylene sulfide. UL-V0 flame retardant.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.62 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0040 - 0.0050 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 25500 psiASTM D638
 8600 psi
@Temperature 204 °C
ASTM D638
 12200 psi
@Temperature 149 °C
ASTM D638
 26000 psi
@Temperature -40.0 °C
ASTM D638
Elongation at Break 1.16 %
@Temperature -40.0 °C
ASTM D638
 1.2 %
@Temperature 22.8 °C
ASTM D638
 1.25 %
@Temperature 204 °C
ASTM D638
 1.35 %
@Temperature 149 °C
ASTM D638
Tensile Modulus 1.15e+6 psi
@Temperature 204 °C
ASTM D638
 1.25e+6 psi
@Temperature 149 °C
ASTM D638
 2.43e+6 psi
@Temperature 22.8 °C
ASTM D638
 2.58e+6 psi
@Temperature -40.0 °C
ASTM D638
Flexural Strength 36000 psiASTM D790
 18400 psi
@Temperature 204 °C
ASTM D790
 23000 psi
@Temperature 149 °C
ASTM D790
 37200 psi
@Temperature -40.0 °C
ASTM D790
Flexural Modulus 900000 psi
@Temperature 204 °C
ASTM D790
 1.10e+6 psi
@Temperature 149 °C
ASTM D790
 2.04e+6 psi
@Temperature 22.8 °C
ASTM D790
 2.17e+6 psi
@Temperature -40.0 °C
ASTM D790
Izod Impact, Notched 6.40 ft-lb/inASTM D256
 6.40 ft-lb/in
@Temperature -40.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 535 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 - 80.0 °C
 140 - 160 °CCavity temperature
Feed Temperature 20.0 - 50.0 °C
Zone 1 285 - 295 °C
Zone 2 290 - 300 °C
Zone 3 295 - 305 °C
Zone 4 300 - 310 °C
Die Temperature 290 - 300 °C
Melt Temperature 300 - 310 °C
Drying Temperature 130 - 140 °C
Dry Time 3.00 - 4.00 hour
Moisture Content 0.020 %Necessary low maximum residual
Dew Point <= -30.0 °CPre-drying
 
Descriptive Properties
Longer pre-drying times/storagelower the temperature to 100° C until processed.<= 60 h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celstran® PPS-GF40-01 AD3002 Black PPS, 40% Glass Reinforced
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose
Techmer ES HiFill® PPS GF40 BK 40% Glass Filled
Omnia Plastica PPS GF40 Polyphenylenesulphide
Techmer ES HiFill® PPS GF40 TL13 40% Glass Filled

PHCR225 / 158794

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.