MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Resin Technology Group TIGA 101-EX Five-Minute Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 1 part resin to 1 part hardener.

TIGA 101-EX is an exceptional epoxy formulation, recommended for lower temperature or wet industrial bonding applications where fast curing is required. This clear, two-part, mild odor, medium- viscosity system mixes easily at room temperature, contains no solvents, and is suitable for high performance structural-bonding applications where the combination of very fast room temperature cure coupled with low shrinkage and excellent mechanical and electrical properties is required. It develops strong, tough bonds to metals, phenolic plastics, polyesters, glass and glass fabrics, hardboards and forestry products, ceramics, rubber, masonry materials, and other construction materials. Fully cured TIGA 101-EX is an excellent electrical insulator and provides superior resistance to vapors and gases, water, galvanic action, petroleum fuels, salt solutions, and many other organic and inorganic compounds.

Applications:

High speed bonding and repairs at low temperatures. Ideal for assembly lines and various production applications such as staking, fillet bonds, and general industrial repairs. Used in component assembly, appliances, electronics, and fiber optics. Sets in five minutes, reaches full strength in about one hour.

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccOf resin
Viscosity 10000 - 16000 cPOf hardener at 25C
 11000 - 15000 cP
@Temperature 25.0 °C
Of resin
 14000 - 17000 cP
@Temperature 25.0 °C
Mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 28Cured 10 minutes at 25°C
 68Cured 30 minutes at 25°C
 74Cured 10 minutes at 60°C
 78 - 82
Shear Strength 2200 - 3200 psiLap
Izod Impact, Notched 2.10 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 415 V/mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Pot Life 3.0 - 5.0 minSmall Mass
 
Descriptive Properties
ColorTransparent, Clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 546S04 Thixotropic UV/Blue Light Cure Adhesive
Tra-Con Tra-Bond 526M02 High Tg Fiber Optic Adhesive
NeXolve Novastrat® 905 Polyimide
CEN® Electronic Material CN Polyimide Film, 1 Mil Thickness

PRESINT629 / 65513

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.