MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta EndurX™ BP15NPN Phenolic Cotton Laminate Sheet
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: Post-forming canvas phenolic material. BP15NPN’s mechanical and electrical properties are similar to BP11EPN. It is made from a cotton fabric weighing more than 4 ounces per square yard and having a thread count of not more than 70 threads per inch in both the warp and filler directions. The binder is a modified phenolic resin system, which permits the material to be heated, formed into a shape and cooled under restraint to hold the newly formed shape.

Key Words: Cotton, Phenolic, Micarta, Post-forming canvas
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Moisture Absorption 4.20 %Condition A; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90ASTM D785
Tensile Strength 6000 psi
@Thickness 3.17 mm
Condition A, Crosswise; ASTM D638
 10000 psi
@Thickness 3.17 mm
Condition A, Lengthwise; ASTM D638
Flexural Strength 14000 psi
@Thickness 1.57 mm
Condition A, Crosswise; ASTM D790
 17000 psi
@Thickness 1.57 mm
Condition A, Lengthwise; ASTM D790
Flexural Modulus 900 ksi
@Thickness 1.57 mm
Condition A, Crosswise; ASTM D790
 1100 ksi
@Thickness 1.57 mm
Condition A, Lengthwise; ASTM D790
Compressive Strength 25000 psi
@Thickness 12.7 mm
Condition A, Flatwise; ASTM D695
Shear Strength 12000 psi
@Thickness 1.57 mm
Condition A, Perpendicular; ASTM D732
Adhesive Bond Strength 1800 psi
@Thickness 12.7 mm
Condition A, Bonding Strength; ASTM D229
Izod Impact, Notched 2.00 ft-lb/in
@Thickness 12.7 mm
Condition E-48/50, Crosswise; ASTM D256
 2.50 ft-lb/in
@Thickness 12.7 mm
Condition E-48/50, Lengthwise; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 350 V/mil
@Thickness 1.57 mm
Condition D-48/50; ASTM D149
 480 V/mil
@Thickness 1.57 mm
Condition A; ASTM D149
Dielectric Breakdown 4000 V
@Thickness 1.57 mm
Condition D-48/50; ASTM D149
 65000 V
@Thickness 1.57 mm
Condition A; ASTM D149
Arc Resistance 10 sec
@Thickness 3.17 mm
Condition A; ASTM D495
Comparative Tracking Index 150 V
@Thickness 3.17 mm
ASTM D3638
 
Thermal PropertiesOriginal ValueComments
UL RTI, Electrical 125 °CUL Bulletin 746b
UL RTI, Mechanical without Impact 125 °CUL Bulletin 746b
Flammability, UL94 HB
@Thickness 1.57 mm
Condition A
 
Descriptive Properties
SubstrateCotton

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNORPM232 / 280548

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.