MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Materion CIROM-IRX™ Cerous Fluoride
Categories: Ceramic; Halide

Material Notes: CIROM-IRX™ is a modified form of cerous fluoride. The material can be handled using standard safety precautions. There is no radioactivity associated with CIROM-IRX™. CIROM-IRX™s manufactured as fully melted ingots at a very high temperature in a controlled atmosphere. The ingot is crushed and sized to lumps, granules or small grains, depending on customer application. Any required particle size range can be produced on short notice.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.20 g/cc0.224 lb/in³
Water Absorption 2.00 - 3.00 %2.00 - 3.00 %2800-3200 and 5600-7300 inm bands
 
Thermal PropertiesMetricEnglishComments
Melting Point 1430 °C2610 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.42
@Wavelength 12000 nm
1.42
@Wavelength 12000 nm
 1.43
@Wavelength 10000 nm
1.43
@Wavelength 10000 nm
 1.44
@Wavelength 8000 nm
1.44
@Wavelength 8000 nm
 1.48
@Wavelength 4000 nm
1.48
@Wavelength 4000 nm
 1.61
@Wavelength 800 nm
1.61
@Wavelength 800 nm
 1.62
@Wavelength 1000 nm
1.62
@Wavelength 1000 nm
 1.64
@Wavelength 600 nm
1.64
@Wavelength 600 nm
 1.66
@Wavelength 400 nm
1.66
@Wavelength 400 nm
IR Transmittance  98.0 %
@Wavelength 11000 nm
98.0 %
@Wavelength 11000 nm
2% Absorption
 98.0 %
@Wavelength 12000 nm
98.0 %
@Wavelength 12000 nm
2% Absorption
 99.0 %
@Wavelength 10600 nm
99.0 %
@Wavelength 10600 nm
1% Absorption
 
Descriptive Properties
ColorTan to brown
Evaporation Temperature1000°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMATER903 / 323501

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.