MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hostacom M2 T02 102942 Polypropylene with 20% Talc Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Hostacom M2 T02 102942 is a 20% talc filled PP homopolymer, with high flowability. The product is available in different color matched pellet form. This grade is delivered in 102942 color version. Applications: Automotive Parts, Under hood

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183-1A
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 33.0 MPaISO 527-1,-2
Flexural Modulus 2700 MPa2mm/min; ISO 178
Charpy Impact, Notched 4.00 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eA
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom X M2 V05 357026 Polypropylene with 20% Talc Filler
LyondellBasell Hostacom M2 N01 L304698 Polypropylene, Mineral Reinforced
LyondellBasell Hostacom M2 N01 102942 Polypropylene with 20% Talc Filler
LyondellBasell Hostacom M2 R18 301105 Polypropylene, Mineral Reinforced
LyondellBasell Hostacom M4 U02 102943 BLK Polypropylene, Mineral Reinforced

PEQT8018 / 219654

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.