MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem Accelerator DCBS
Categories: Other Engineering Material

Material Notes: Product Description: Accelerator DCBS is a delayed action sulfenamide accelerator for use in natural and synthetic rubbers. It is recommended for applications where exceptionally long flow times are required. DCBS is particularly suitable for rubber goods subjected to high dynamic stresses. It is a primary accelerator which can be used alone or in combination with many secondary accelerators. DCBS offers the best scorch resistance of all commonly used sulfenamide accelerators.

Application: DCBS is very effective for use in thick cross-section molded articles. It also is finds application where high processing temperatures are encountered or delayed cures are needed for optimum adhesion. Total curing times are longer than with other sulfenamides, but the flow time/curing time ratio is favorable. DCBS is also employed in conveyor belts, driving belts, shock absorbers, mountings and other intricately shaped molded goods requiring extremely long flow periods in the molding process. The use of zinc oxide is necessary and stearic acid should be included in compounds where high modulus values are required.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/cc
Volatiles <= 0.40 %
Ash <= 0.30 %
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 96.0 °C
 
Descriptive Properties
Appearancebuff granules
Assay>95%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH442 / 315360

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.