MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUTENE-H XL1800 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Description: LUTENE-H XL 1800 is a optimum materials for under-floor heating and drinking water pipe by RAM type extrusion. It is excellent product with long-term internal pressure creep property and crosslinked property, mechanical properties

Applications: Peroxide crosslinked pipes for under-floor heating and drinking water

CAS No. 9002-88-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/ccASTM D1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength, Yield 23.5 MPa3410 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Flexural Modulus 0.981 GPa142 ksiASTM D790
Izod Impact, Unnotched >= NB
@Temperature 23.0 °C
>= NB
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Crystallization Temperature 129 °C264 °FMelting; DSC
Vicat Softening Point 123 °C253 °FASTM D1525
Brittleness Temperature <= -80.0 °C<= -112 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis HE1878E High Density Polyethylene Powder for Crosslinked Pipes
Borealis HE1878 High Density Polyethylene Powder for Crosslinked Pipes
LG Chemical SEETEC PB150 HDPE
LG Chemical SEETEC PM360 HDPE
SIDPEC EGYPTENE® HD 5420 GA HDPE Blow Molding

PLAY202 / 148212

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.