MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol ESTALOC® 59200 Ester-Type, Reinforced Engineering Thermoplastic
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Glass Filled

Material Notes: Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extension to the Noveon Estane® TPU technology, Estaloc® RETP products complement Estane's durability and aesthetics with increased stiffness capability and dimensional stability over a broad temperature performance range not available from other engineering thermoplastics.

Major Benefits of Estaloc® RETPs:

  • Superior Dimensional Stability approaching that of metals
  • Class A surface aesthetics
  • Paintability with no primer nor adhesion promoter
  • Excellent abrasion and scuff/mar resistance
  • Toughness over a broad temperature range
  • Excellent adhesion to a variety of overmolding chemistries

Information provided by Noveon, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.44 g/ccISO 1183
Filler Content 30 %
Linear Mold Shrinkage 0.0015 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 68ISO 868
Tensile Strength, Ultimate 74.0 MPaISO 527-2/1A/5
Elongation at Break 20 %ISO 527-2/1A/5
Tensile Modulus 2.883 GPaISO 527-2/1A/1
Flexural Strength 67.0 MPaISO 178
Flexural Modulus 2.36 GPaISO 178
Izod Impact, Notched (ISO) 25.0 kJ/m²Low Temp; ISO 180/1eA
 70.0 kJ/m²ISO 180/1eA
Izod Impact, Unnotched (ISO) NBISO 180/1eU
 95.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1eU
Charpy Impact Unnotched 14.4 J/cm²ISO 179/1eU
 103 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 5.80 J/cm²ISO 179/1eA
 2.00 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
Taber Abrasion, mg/1000 Cycles 20CS-17 wheel; ASTM D1044
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.5 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 154 °Cmethod Bf; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 126 °Cmethod Af; ISO 75-2
Vicat Softening Point 107 °Ctemperature B; ISO 36
 176 °Ctemperature A; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTALOC® 59300 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Lubrizol ESTALOC® 59104 Ester-Type, Reinforced Engineering Thermoplastic
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Kingfa JH960 HT10 Non-halogenated Flame Retardant PC/ABS Alloy
Lubrizol ESTALOC® 59600 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane

PNOVEON073 / 55338

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.