MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Akrochem PROAID® RW Process Aids
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Akrochem’s Proaid RW is a carefully selected blend of resins and waxes, thus RW. Proaid RW is water-free, filler-free and designed to act as an economical processing aid for all natural and synthetic rubber compounds. Proaid RW reduces compound viscosity, improves mold flow (compression, transfer and injection) and release from all metal surfaces with minimal affect on cured physical properties in most compounds.

Applications: The dosage for Proaid RW is 1 to 4 phr, depending on the polymer and the process. Due to the wax constituent, Proaid RW has the tendency to bloom at about 5 phr. The loading to which bloom may occur is dependant on the rubber compound. The very low water content creates fewer problems in high temperature cures (like CV cures). Also, no fillers (no ash) have been added which means Proaid RW is more concentrated. All materials that makeup Proaid RW previously have been acceptable by the FDA (per CFR 21 177.2600 or 175.105). Proaid RW may be used to improve: mold filling and cured part finish, flow characteristics in molding operations, release from molds, mills and internal mixers, dispersion of fillers during mixing (add early in mix) and reduce mold fouling.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/cc
 
Thermal PropertiesMetricEnglishComments
Melting Point 155 °C311 °F
 
Descriptive Properties
Appearancered pastilles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH366 / 315284

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.