MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Resinlab® RC8080 Anaerobic Retaining Compound
Categories: Polymer; Adhesive

Material Notes: The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products form a tough permanent bond which greatly enhances the torque and pullout strength. They are single component solvent free materials manufactured in a wide variety of viscosities and setting times to satisfy specific bonding applications. This technology increases the reliability and performance of assemblies while reducing dependence upon maintaining costly tight machining tolerances.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/cc
Viscosity 1400 cP
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 4200 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °C
Minimum Service Temperature, Air -65.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 minFixture
 8.00 hourFull Cure
 
Descriptive Properties
ColorGreen
Gap Fill (mil)15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resinlab® RC8020 Anaerobic Retaining Compound
Resin Technology Group EN 239-2 Cationic UV Cure Epoxy Adhesive
Resin Technology Group DP031199-1 Cationic UV Cure Epoxy Adhesive
Epoxy Technology EPO-TEK® 314 Thermally and Electrically Insulating Epoxy

PRESL170 / 101584

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.