MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Huber Martinal® TM-3620 Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Martinal® TM-3620 aluminum hydroxide is a thermally conductive material designed to be used either by itself or in blends with other fillers to obtain high loadings in epoxy, polyurethane and silicone-based gap-fillers.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.40 g/cc2.40 g/cc
Bulk Density 1.20 g/cc0.0434 lb/in³
Moisture Absorption <= 0.250 %
@Temperature 105 °C
<= 0.250 %
@Temperature 221 °F
Particle Size 100 µm100 µmd90, laser scattering, Cilas
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.581.58
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 34.5 %
@Temperature 1200 °C
34.5 %
@Temperature 2190 °F
Na2O <= 0.030 %<= 0.030 %soluble
 
Descriptive Properties
Al(OH)3 (%)99.6
FunctionalityThermal Conductivity
Market/Application: ThermoplasticsYes
Market/Application: ThermosetsYes
Market/Application: TransportationLithium-Ion Battery Gap Fillers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER744 / 300850

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.