MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF Ultradur® B 4560 BK10089 PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Ultradur B 4560 BK10089 is an injection molding, pigmented black, PBT grade.

Applications: Typical applications include industrial parts in the automotive field, such as head lamp bezels

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Viscosity Test 112 cm³/g1.12 dl/gISO 1628
Linear Mold Shrinkage, Flow 0.015 cm/cm0.015 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cm0.020 in/inISO 294-4
Melt Flow 33 g/10 min
@Load 2.16 kg,
Temperature 250 °C
33 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psiISO 527
Elongation at Break 35 %35 %Nominal; ISO 527
Elongation at Yield 4.0 %4.0 %ISO 527
Tensile Modulus 2.60 GPa377 ksiISO 527
Charpy Impact Unnotched  8.50 J/cm²
@Temperature -30.0 °C
40.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 14.0 J/cm²
@Temperature 23.0 °C
66.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 100 - 120 °C
@Time 14400 sec
212 - 248 °F
@Time 4.00 hour
Moisture Content <= 0.040 %<= 0.040 %
Injection Pressure 3.45 - 10.3 MPa500 - 1500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8913 / 254871

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.