MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Reynolds Feather Lite® Lightweight Urethane Casting Resin
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: Feather Lite™ is a heavily filled low-density urethane casting resin. Cured plastic is lightweight (it floats in water!) and has a much lower density than other casting resins. Feather Lite™ features a convenient 1A:1B by volume mix ratio and mixes easily (pre-mixing of parts A & B is necessary). Cured plastic is strong and can be carved, machined, drilled, sanded, etc. Feather Lite™ can be pigmented with SO-Strong™ color tints prior to casting and finished castings can be painted. And because this product is low-density, it yields more plastic per pound/kg. than other casting resins, the cost per casting is low. Feather Lite™ can be used for a variety of art or industrial design related applications including reproducing sculpture, making fishing lures, prototype model making, casting doll heads and figures, etc.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.670 g/cc0.670 g/ccASTM D-1475
Viscosity 410 cP410 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5858ASTM D-2240
Tensile Strength, Ultimate 14.9 MPa2160 psiASTM D-638
Elongation at Break 1.6 %1.6 %ASTM D-638
Tensile Modulus 1.08 GPa156 ksiASTM D-638
Flexural Strength 23.7 MPa3440 psiASTM D-790
Flexural Modulus 1.133 GPa164.3 ksiASTM D-790
Compressive Strength 21.2 MPa3070 psiASTM D-695
Compressive Modulus 0.370 GPa53.7 ksiASTM D-695
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 60.0 °C140 °FASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min2.00 hourHandling Time
Pot Life 8.50 min8.50 minASTM D-2471
 
Descriptive Properties
ColorBeige
Mix Ratio1A:1Bby volume
 1A:1Bby weight
Specific Volume41.3[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN045 / 296746

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.