System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Aaron Industries AVPE HD 300-3 MELT 20 Virgin Polyethylene
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Low Density (LDPE)
;
Low Density Polyethylene (LDPE), Blow Molding Grade
Material Notes:
A natural HDPE resin, specifically designed for high speed blow molding and extrusion applications.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
0.955
g/cc
ASTM D792
Linear Mold Shrinkage
0.0040
in/in
ASTM D955
Melt Flow
20
g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
3800
psi
ASTM D638
Flexural Modulus
320
ksi
ASTM D790
Izod Impact, Notched
1.00
ft-lb/in
ASTM D256
Thermal Properties
Original Value
Comments
Vicat Softening Point
185
°F
ASTM D1525
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
NIZHNEKAMSKNEFTEKHIM PE 2062x (62135) High Density Polyethylene
NIZHNEKAMSKNEFTEKHIM PE 2060V (60118) High Density Polyethylene
LG Chemical LUTENE-H BE0350 HDPE
Eastman M3018-P Polyethylene
DuPont 20 Series 2020 Specialty Polyethylene Resin
PRONAA980 / 135311
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.