MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Henkel Loctite® Shadowcure™ 397 Acrylic/urethane Heat Cure Coating
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes:
Conformal Coatings
Conformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Loctite offers both acrylic/urethane and silicone conformal coatings which are cured by UV, heat, or a two-part cure mechanism.

Loctite® 397 Shadowcure™ Acrylic/urethane Heat Cure Coating
Designed to replace historic solvent based heat cure coatings in high reliability applications. No solvents. Low VOC. Cure Type: Heat or Catalytic MIL-I-46058C Approved; UL-746C Approved; IPC-CC-830A Approved; Bellcore TR-NWT-000078 Pending Approval.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 450 cP450 cP(mixed)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ASTM D2240
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 2.00e+16 ohm2.00e+16 ohmASTM D257
Dielectric Strength 33.9 kV/mm860 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min0.167 hourPrimary Cure is Heat: Full Cure in 10 minutes at 100C. Secondary Cure is Catalytic: Full Cure in 2-5 days without heat, or more than 24 hours at ambient temp.
 
Descriptive Properties
Capillary Flow25 secTime to flow 0.5" @ 100°C through a gap of 0.001"
ColorClear/Purple (cured)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOCT174 / 51910

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.