MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: ALATHON M6080 is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include cases, tote bins, crates and trays and open-head pails.

Regulatory Status: M6080 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.

Specific recommendations for processing M6080 can only be made when the processing conditions, equipment and end use application are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.593 - 0.625 g/ccASTM D1895
Density 0.960 g/ccASTM D1505
Melt Flow 7.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Spiral Flow 8.60 inEquistar test
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70ASTM D2240
Tensile Strength at Break 2300 psi50 mm/min; ASTM D638
Tensile Strength, Yield 4250 psi50 mm/min; ASTM D638
Elongation at Break 380 %50 mm/min; ASTM D638
Tensile Modulus 122600 psi1% Secant; 50mm/min; ASTM D638
 146400 psi50mm/min; ASTM D638
Flexural Modulus 205100 psi12.5 mm/min; ASTM D790
 155400 psi
@Strain 2 %
Secant; 12.5 mm/min; ASTM D790
Flexural Modulus, 1% Secant 190200 psi2.5 mm/min; ASTM D790
Izod Impact, Notched 1.40 ft-lb/inASTM D256
 NB
@Temperature -18.0 °C
ASTM D4812
 
Thermal PropertiesOriginal ValueComments
Melting Point 270.9 °FASTM D3418
Crystallization Temperature 115.9 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °CASTM D648
Brittleness Temperature <= -76.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 450 °F
Middle Barrel Temperature 470 °F
Front Barrel Temperature 475 °F
Nozzle Temperature 475 °F
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade
Ethydco Advancene™ EM-5204-UVH High Density Polyethylene Resin
Ethydco Advancene™ EM-6308-UV High Density Polyethylene Resin
Flint Hills P6G2N-095 Impact Copolymer Polypropylene
Ineos L12Z-01 Polypropylene Impact Copolymer

PEQU0797 / 104153

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.