MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
3D Systems DuraForm® AF Nylon for SLS® Systems
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Polyamide (nylon) material with metallic appearance for real-world physical testing and functional use. For use with all selective laser sintering SLS® systems.

    Applications
  • Housings and enclosures
  • Consumer products
  • Appropriate for low- to mid-volume rapid manufacturing
  • Parts requiring machining or joining with adhesives
  • Complex production and prototype plastic parts
  • Form, fit or functional prototypes
  • Parts requiring stiffness
  • Thermally stressed parts
  • Plastic parts requiring a metallic appearance

All information provided by 3D Systems.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 0.690 g/cc
 0.890 g/cc
@Temperature 25.0 °C
tap
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ASTM D2240
Tensile Strength, Ultimate 35.0 MPaASTM D638
Elongation at Break 1.5 %ASTM D638
Tensile Modulus 3960 MPaASTM D638
Flexural Strength 44.0 MPaASTM D790
Flexural Modulus 3517 MPaASTM D790
Izod Impact, Notched 58.7 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched 1.23 J/cm
@Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.60e+13 ohm-cmASTM D257
Surface Resistance 6.00e+12 ohmASTM D257
Dielectric Constant 14.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 1.80 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 109 µm/m-°C
@Temperature 35.0 - 172 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 180 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 137 °CASTM D648
 
Descriptive Properties
AppearanceLight grey metallic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3D Systems DuraForm® PA Nylon for SLS® Systems
3D Systems DuraForm® HST Fiber Filled Nylon for SLS Systems
3D Systems DuraForm® GF Glass Filled Nylon
3D Systems CastForm™ PS Plastic for SLS® Systems
3D Systems DuraForm® Flex Thermoplastic Elastomer for SLS® Systems

PAPPR120 / 83499

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.