MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® OG116-31 UV Cure Optical Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Description: EPO-TEK® OG116-31 is a single component, UV curable epoxy adhesive and encapsulant, designed for PCB and circuit assembly applications found in semiconductor, computer, medical, and scientific/OEM industries.

Advantages & Application Notes:

  • Viscosity/rheology adapted to high volume syringe needle dispensing with no tailing.
  • Complies with USP Class VI biocompatibility standards.
  • Versatility in cure. Product responds to a broad range of UV light, and secondary thermal post-curing.
  • Suggested applications:
    • Semiconductor: COB glob top covering IC’s and wire bonds; glob top dam; encapsulating and sealing; adhesion to FR4, Kapton, silicon.
    • Fiber Optic: making fiber optic pigtails; active alignment of optics; adhesion to many types of glass, metals, ceramics and plastics.
    • Opto-electronic:
      • Perimeter/main seal for LCD’s, compatible with VAN liquid crystal for LCoS devices.
  • High Tg and low outgassing are indicative of its high temperature performance.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/cc
Particle Size <= 20 µm
Viscosity 20000 - 30000 cP
@Temperature 23.0 °C
10 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83
Tensile Modulus 264000 psiStorage
Shear Strength 3400 psiDie
 
Thermal PropertiesOriginal ValueComments
CTE, linear 41.0 µm/m-°CBelow Tg
 170 µm/m-°CAbove Tg
Maximum Service Temperature, Air 200 °CContinuous
 300 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 115 °CDynamic Post- Cure Scan 20—200°C; Ramp -10—200°C @ 20°C/Min
Decomposition Temperature 409 °CDegradation Temperature
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.5662
@Wavelength 589 nm
Transmission, Visible >= 92 %
@Wavelength 500 nm
Spectral
 >= 96 %
@Wavelength 660 - 1640 nm
Spectral
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
ColorCloudy Whitebefore cure
ConsistencyViscous liquid
Number of ComponentsSingle
Thixotropic Index1.3
Weight Loss0.31%200°C
 0.68%250°C
 1.18%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® OG603 UV Cure Optical Epoxy
Epoxyset Epoxiohm EO-98HT Electrically Conductive Epoxy Adhesive
G-11 Fiberglass Epoxy Laminate Sheet
Epoxy Technology EPO-TEK® OG198-54 UV Cure Optical Epoxy
Overview of materials for Epoxy/Carbon Fiber Composite

PPOXYT164 / 141203

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.