MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Nitriflex Nitrilatex LVP-106 Vinyl Pyridine Styrene Butadiene Latex
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid.

Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesives manufacture, fibers agglomeration, supported gloves manufacture, impregnation of non-woven, etc.

Information provided by Dax Resinas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 40 - 42 %Method L-001/P-065; ASTM D1417
pH 10 - 1125°C, Method L-003; ASTM D1417
Brookfield Viscosity 45 - 54 cP(spindle=1, 20 rpm); ASTM D1417
Mooney Viscosity 30 - 45Method L-015; ASTM D1417, ASTM D1646
Surface Tension 46 - 55 dynes/cmMethod L-005/L-040; ASTM D1417
 
Descriptive Properties
AppearancePurple Liquid
Coagulum Content %0-0.05ASTM D1417; Method L-004
Cream Content g/150ml0-0.03Method L-013
Vinyl Pyridine Content g/150ml13-15ASTM D3533; Method B-016/B-028

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Armacell Ensolite™ MLC-Black PVC/NBR
Chlorosulfonated Polyethylene Rubber (CM, CSM)
Chosun Refractories CFA-2 Ceramic Foam
DuPont Mobility and Materials AquaStik® AQS-2900 Polychloroprene Latex
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced

PDAX069 / 29494

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.