MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NovaCentrix Metalon® ICI-021 Copper Oxide Screen Ink – Aqueous dispersion
Categories: Fluid; Other Engineering Material

Material Notes: ICI-021 is a copper oxide ink which is chemically reduced post-printing into metallic copper by processing with PulseForge® tools. ICI-021 is designed to produce conductive traces on porous, low temperature substrates such as paper. ICI-021 ink is specially formulated for screen printing.

Metalon ICI-021 when printed and cured, produces conductive traces. ICI-021 prints MUST be processed by PulseForge® tools from NovaCentrix to become conductive. Thermal curing is not applicable. Printed traces of ICI-021 are not conductive prior to processing with PulseForge tools.

Sheet resistance as low as 20 milliohm/square is achievable on paper using a 165 mesh screen.

Print Information

  • Substrate: Paper (Exact® Index – 110 lb. – Wausau Paper)
  • Printer: Flat-bed manual screen printer (165 mesh screen)
  • Post-Process Tool: PulseForge® 3200 or 3300
  • Environment: Atmosphere – no special preparation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.00 g/cc2.00 g/cc
Particle Size 250 µm250 µmz-avg by DLS
Brookfield Viscosity 300000 cP300000 cPSpindle LV#4; 1.5 rpm
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 0.020 ohm>= 0.020 ohmExample; on paper with 165 mesh screen
 
Descriptive Properties
CuO Content (wt%)57.5
Flash pointNon-flammable
General DescriptionWater-based copper oxide ink

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NovaCentrix HPS-030AE1 Silver Aerosol Ink
NovaCentrix PSPI-1000® Conductive Aerosol Spray Ink
Copper (II) Oxide, CuO (Tenorite)
American Elements Copper Oxide Nanopowder
Morgan Advanced Ceramics Z500 MgO Stabilized Zirconia

ENOVA913 / 191523

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.