MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Prime Polymer ULTZEX® 1520L LLDPE, Film
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Advantages: Heat Seal Strength; Low Temp Heat Seal

Major Applications: Lamination Film

Information provided by Prime Polymer Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.914 g/ccJIS K7112
Environmental Stress Crack Resistance >= 1000 hourASTM D1693
Melt Flow 2.3 g/10 minJIS K7210
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 54JIS K7215
Tensile Strength at Break 18.0 MPaJIS K7161
Elongation at Break 430 %Nominal; JIS K7161
Modulus of Elasticity 0.150 GPaJIS K7171
Charpy Impact, Notched NBJIS K7111
 
Thermal PropertiesOriginal ValueComments
Melting Point 115 °CJIS K7121
Vicat Softening Point 98.0 °CJIS K7206

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRIME023 / 313416

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.