Pro-fax EP349U high flow polypropylene impact copolymer is available in pellet form. This resin is typically used in thin-wall injection molding applications and offers very good low temperature impact resistance. Applications: House wares, Sports, Leisure & Toys, TWIM Food ContainersInformation provided by LyondellBasell. |