MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mo-Sci Corporation GL-0275-S Class VI Soda-Lime Spheres  (discontinued **)
Categories: Ceramic; Glass; Oxide; Silicon Oxide

Material Notes: Appearance: Solid soda-lime glass microspheres with light green color in powder form.

Typical applications of GL0275-S beads including: high temperature spacer material for gauge control, coating, filler for plastic, retroreflection applications and etc.

Information provided by Mo-Sci Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.30 g/cc0.0470 lb/in³of Dry Beads
Density 2.50 g/cc0.0903 lb/in³
pH 7.87.8in water
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 30.0 - 300 °C
5.00 µin/in-°F
@Temperature 86.0 - 572 °F
Softening Point 650 °C1200 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 0.00 - 5.0 %0.00 - 5.0 %
CaO 6.0 - 15 %6.0 - 15 %
Fe2O3 <= 0.80 %<= 0.80 %
MgO 1.0 - 5.0 %1.0 - 5.0 %
Na2O 10 - 20 %10 - 20 %
SiO2 65 - 75 %65 - 75 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Mo-Sci Corporation GL-0191 Soda-Lime Glass Spheres
H.C. Starck Standard 120 Titanium Carbide, TiC
Mo-Sci Corporation GL-0191-S Soda-Lime Glass Spheres
Silicon Carbide, Alpha SiC

CMOSCI027 / 137210

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.