MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Kaolite® 1:2:4 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Crystalline Silica. Cast / Gun installation. Kaolite 1:2:4 is a general-purpose, cast/gun lightweight monolithic for use up to 2000°F (1093°C). It provides the advantage of a pre-mixed, controlled formula product compared to typical 1:2:4 spec field mixes.

Applications:

  • Backup insulation in two component linings in petrochemical process units
  • Hot face lining in ductwork from waste heat recovery boilers and process unit
  • F.C.C.U. linings-regenerator
  • Hydrogen or reducing atmosphere linings
  • Radiant section in steam flood generators
  • Hydrogen or reducing atmosphere linings
  • Steam flood generator convection sections and target walls.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.801 - 0.961 g/cc
@Temperature 816 °C
fired; ASTM C 134
 0.881 - 1.057 g/cc
@Temperature 104 °C,
Time 86400 sec
dried; ASTM C 134
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.000520 - 0.00103 GPa
@Temperature 1093 °C,
Time 18000 sec
fired; ASTM C133
 0.000550 - 0.00121 GPa
@Temperature 816 °C,
Time 18000 sec
fired; ASTM C133
 0.000860 - 0.00138 GPa
@Temperature 104 °C,
Time 86400 sec
dried; ASTM C133
Compressive Strength 1.70 - 3.10 MPa
@Temperature 816 °C,
Time 18000 sec
Cold Crushing Strength, fired; ASTM C133
 1.70 - 3.10 MPa
@Temperature 1093 °C,
Time 18000 sec
Cold Crushing Strength, fired; ASTM C133
 2.06 - 3.50 MPa
@Temperature 104 °C,
Time 86400 sec
Cold Crushing Strength, dried; ASTM C133
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.140 W/m-K
@Temperature 260 °C
ASTM C201
 0.220 W/m-K
@Temperature 538 °C
ASTM C201
 0.270 W/m-K
@Temperature 815 °C
ASTM C201
Maximum Service Temperature, Air <= 1093 °C
Shrinkage 0.00 - 0.20 %
@Treatment Temp. 104 °C,
Time 86400 sec
dried
 0.40 - 1.0 %
@Treatment Temp. 816 °C,
Time 18000 sec
fired
 
Processing PropertiesOriginal ValueComments
Moisture Content 55 - 65 %casting by vibrating
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
Al2O3 26 %
CaO 17 %
Fe2O3 11 %
K2O+Na2O 2.6 %Na2O & K2O
MgO 3.4 %
SiO2 38 %
TiO2 1.4 %
 
Descriptive Properties
Placement, average (kg)913to place 1m3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaolite® 1800 Thermal Ceramic, Cast installation

CMORF6352 / 203136

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.