MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Xantar® C CM 406 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: XANTAR® C properties are: Highest flow in combination with excellent toughness. High level of purity. High stability. Bright natural color. The benefits are: easier filling of complex parts, lower mould deposit during injection molding, low volatiles level and reduced fogging tendency, better long-term property retention and improved color consistency and appearance.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Melt Density 1.01 g/cc
@Temperature 280 °C
Water Absorption 0.60 %Sim. To ISO 62
Moisture Absorption 0.200 %
Linear Mold Shrinkage, Flow 0.0060 cm/cmISO 294-4
Melt Flow 24 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 MPaISO-527-1,2
Elongation at Break >= 50 %ISO 527-1,2
Elongation at Yield 4.0 %ISO 527-1,2
Tensile Modulus 2200 MPaISO 527-1,2
Flexural Strength 80.0 MPaISO 178
Flexural Modulus 2250 MPaISO 178
Izod Impact, Notched (ISO) 35.0 kJ/m²
@Temperature -40.0 °C
ISO 180/4A
 55.0 kJ/m²
@Temperature -20.0 °C
ISO 180/4A
 65.0 kJ/m²
@Temperature 23.0 °C
ISO 180/4A
Charpy Impact Unnotched 40.0 kJ/m²ISO 179/1eU
 20.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 35.0 kV/mmIEC 60243-1
Comparative Tracking Index 275 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°CISO 11359,1-2
CTE, linear, Transverse to Flow 70.0 µm/m-°CISO 11359-1,2
Specific Heat Capacity 2.28 J/g-°Cmelt
Thermal Conductivity 0.230 W/m-Kmelt
Deflection Temperature at 1.8 MPa (264 psi) 105 °CISO 75-1,2
Vicat Softening Point 120 °C
@Load 5.10 kg
rate 50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695, 11-10
 HB
@Thickness 3.00 mm
IEC 60695, 11-10
Oxygen Index 22 %ISO 4589, 1-2
Glow Wire Ignition Temperature 700 °C
@Thickness 1.50 mm
IEC 60695-2-13
 700 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 675 °C
@Thickness 1.50 mm
IEC 60695-2-12
 675 °C
@Thickness 1.50 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CAs Tested; Injection; ISO 294
Mold Temperature 70.0 °CAs Tested; Injection; ISO 10724
Ejection Temperature 95.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo PULSE™ 2000 EZ PC/ABS Engineering Resin
Avient Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE)
BASF Elastollan® C 70 A HPM TPUR
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer

PMITSU9346 / 192010

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.