MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

UBE Upilex® 25VT Polyimide Film
Categories: Polymer; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: UPILEX®-VT and UPILEX®-NVT are heat bonding polyimide films having heat fusing layers on both side of the film, created by the polyimide resin equivalent of UPILEX®-S. High quality flexible circuits without an adhesive layer are obtained, by heating and pressing UPILEX®-VT or UPILEX®-NVT with metal (Cu, SUS, Al) foil. In addition, they are also available for bonding films comprised of metal, ceramic and other materials. Flexible circuits without adhesive are produced. This offers high tensile strength and tear strength. Offering the same low water absorption, low dimensional change and high heat resistance as UPILEX®-S, with the addition of laminate workability in the heat press.

Information provided by UBE Industries, LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ASTM D1505-03
Water Absorption 1.1 %1.1 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 530 MPa76900 psiASTM D882
Elongation at Break 90 %90 %ASTM D882
Tensile Modulus 7.50 GPa1090 ksiASTM D882
Tear Strength 3.00 kN/m17.1 pliIPC-TM-650 2.4.17.1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmDC 100V; ASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmDC 100V; ASTM D257
Dielectric Constant  3.2
@Frequency 1e+9 Hz
3.2
@Frequency 1e+9 Hz
Triplate-Line Resonator
 3.2
@Frequency 1e+10 Hz
3.2
@Frequency 1e+10 Hz
Triplate-Line Resonator
Dielectric Strength 7.20 kV/mm
@Frequency 60 Hz
183 kV/in
@Frequency 60 Hz
ASTM D149
Dissipation Factor  0.0050
@Frequency 1e+9 Hz
0.0050
@Frequency 1e+9 Hz
Triplate-Line Resonator
 0.0070
@Frequency 1e+10 Hz
0.0070
@Frequency 1e+10 Hz
Triplate-Line Resonator
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C
@Temperature 50.0 - 300 °C
11.1 µin/in-°F
@Temperature 122 - 572 °F
Fine linear dilatometer
Decomposition Temperature 584 °C1080 °FTG-DTA. In air. @ 5% wieght loss
Flammability, UL94 V-0V-0
Shrinkage 0.31 %
@Temperature 300 °C,
Time 7200 sec
0.31 %
@Temperature 572 °F,
Time 2.00 hour
heat; JIS C2318

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUBD9851 / 287314

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.