MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
AISI Type S21900 (21-6-9) Stainless Steel, annealed sheet and strip
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T S20000 Series Stainless Steel

Material Notes: Austenitic, high strength, excellent corrosion resistance, and low magnetic permeability. Applications include aircraft applications such as ducting and bellows systems, tail pipes and exhaust systems, clamps, fasteners, flanges, and hydraulic tubing.

Key Words: UNS S21900, AMS 5561, ASTM A269 (XM-10), ASTM A276 (XM-10), ASTM A314 (XM-10), ASTM A412 (XM-10), ASTM A473 (XM-10), ASTM A580 (XM-10)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.83 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 765 MPa
 354 MPa
@Temperature 705 °C
 416 MPa
@Temperature 650 °C
 467 MPa
@Temperature 595 °C
 490 MPa
@Temperature 540 °C
 518 MPa
@Temperature 480 °C
 549 MPa
@Temperature 425 °C
 594 MPa
@Temperature 315 °C
 616 MPa
@Temperature 205 °C
 693 MPa
@Temperature 95.0 °C
Tensile Strength, Yield 444 MPa
@Strain 0.2 %
 184 MPa
@Strain 0.2 %,
Temperature 650 °C
 185 MPa
@Strain 0.2 %,
Temperature 705 °C
 193 MPa
@Strain 0.2 %,
Temperature 595 °C
 202 MPa
@Strain 0.2 %,
Temperature 480 °C
 203 MPa
@Strain 0.2 %,
Temperature 540 °C
 221 MPa
@Strain 0.2 %,
Temperature 425 °C
 259 MPa
@Strain 0.2 %,
Temperature 315 °C
 289 MPa
@Strain 0.2 %,
Temperature 205 °C
 353 MPa
@Strain 0.2 %,
Temperature 95.0 °C
Elongation at Break 42.5 %in 50 mm
 24 %
@Temperature 705 °C
in 50 mm
 26 %
@Temperature 650 °C
in 50 mm
 30 %
@Temperature 595 °C
in 50 mm
 33 %
@Temperature 315 °C
in 50 mm. Broke on gage mark.
 33 %
@Temperature 425 °C
in 50 mm. Broke on gage mark.
 35 %
@Temperature 540 °C
in 50 mm
 40 %
@Temperature 205 °C
in 50 mm
 41 %
@Temperature 480 °C
in 50 mm
 41.5 %
@Temperature 95.0 °C
in 50 mm
Modulus of Elasticity 200 GPaTypical for stainless steel
Machinability 30 %Based on 100% machinability for AISI 1212 steel.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000730 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.7 µm/m-°C
@Temperature 25.0 - 95.0 °C
 17.3 µm/m-°C
@Temperature 25.0 - 205 °C
Annealed
 18.2 µm/m-°C
@Temperature 25.0 - 315 °C
Annealed
 19.1 µm/m-°C
@Temperature 25.0 - 540 °C
 20.0 µm/m-°C
@Temperature 25.0 - 760 °C
Annealed
 20.0 µm/m-°C
@Temperature 25.0 - 870 °C
Annealed
 20.5 µm/m-°C
@Temperature 25.0 - 980 °C
Annealed
Specific Heat Capacity 0.480 J/g-°CTypical value for stainless steel.
Thermal Conductivity 7.80 W/m-K
@Temperature -180 °C
 10.9 W/m-K
@Temperature -73.0 °C
 13.8 W/m-K
@Temperature 95.0 °C
 16.1 W/m-K
@Temperature 205 °C
 18.2 W/m-K
@Temperature 315 °C
 20.2 W/m-K
@Temperature 425 °C
 22.5 W/m-K
@Temperature 540 °C
 24.7 W/m-K
@Temperature 650 °C
 26.8 W/m-K
@Temperature 760 °C
 28.9 W/m-K
@Temperature 870 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 20 %
Iron, Fe 64 %
Manganese, Mn 9.0 %
Nickel, Ni 6.0 %
Nitrogen, N 0.23 %
Phosphorus, P <= 0.060 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type 317L Stainless Steel, annealed tubing
AISI Type 304HN Stainless Steel, Annealed Sheet , Strip
AISI Type T15 Tungsten High Speed Tool Steel (UNS T12015)
AISI Type T1 Tungsten-Alloy High-Speed-Tool Steel (UNS T12001)
AISI Type S7 Tool Steel (UNS T41907)

MQM22AM / 13644

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.