MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Taiwan PU Corporation TPUI-G98 High Wear Resistance, Injection Molding Polycaprolactone Base TPU
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection Molding

Information provided by Taiwan PU Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 98
Tensile Strength at Break 44.13 MPa
Elongation at Break 550 %
100% Modulus 0.0127 GPa
@Strain 100 %
300% Modulus 0.0206 GPa
@Strain 300 %
Resilience 65%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 6.0
 
Processing PropertiesOriginal ValueComments
Feed Temperature 195 °C
Middle Barrel Temperature 200 °CCompress zone
Front Barrel Temperature 205 °CMetering zone
Adapter Temperature 210 °C
Die Temperature 410 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Taiwan PU Corporation TPUI-G90 High Wear Resistance, Injection Molding Polycaprolactone Base TPU
Taiwan PU Corporation TPUI-E98 General Grade, Injection Molding Polyester Base TPU

PTPU32 / 70888

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.