MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Solvay XMTM54FRB (EF4511) Epoxy Resin Matrix
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: XMTM54FRB (EF4511) is a black pigmented, flame-retarded, 120°C curing epoxy resin matrix. This resin has been specifically designed for use in the DForm® product format and is particularly suited to the automotive industry from both structural and body panel applications. XMTM54FRB (EF4511) is suitable for autoclave and press molding processes. After an optional post-cure, this material can generate a glass transition temperature of 150°C.

Features & Benefits:

  • 30 days out life at 21°C (70°F)
  • 12 months storage at -18°C(0°F)
  • 120°C (248°F) initial cure
  • Rapid cure-15 minutes at 140°C (248°F)
  • Resin optimized for DForm prepreg format

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³Cured resin, 1 hr at 120°C
Storage Temperature -18.0 °C-0.400 °F
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 102 °C216 °FDMA E' onset Tg, 1 hr at 120°C, wet
 125 °C257 °FDMA E' onset Tg, 1 hr at 120°C, dry
 140 °C284 °FDMA E' onset Tg, 15 mins at 140°C press cure, dry
 150 °C302 °FDMA E' onset Tg, 1 hr at 120°C + 2 hrs at 150°C, dry
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay MTM® 49-3 Epoxy Prepreg with 36% M46J-124 Carbon Fiber

PCYTED147 / 180449

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.