MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 95 E 4861 Polyester-Based TPU-Injection Extrusion Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Introduction: IROGRAN A95 4861 is a high performance polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN A95E 4861 is part of the HUNTSMAN technical extrusion product range and offers a specially designed, flexible material with a broad processing window particularly suitable for the preparation of extruded films.

Performance Features:

  • Excellent hydrolysis resistance
  • High crystallization rate
  • Good low temperature flexibility
  • Good processability

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccASTM D792
Linear Mold Shrinkage 0.011 in/inASTM D995
Melt Index of Compound 45 g/10 min
@Load 21.6 kg,
Temperature 215 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 96ASTM D2240
Hardness, Shore D 54ASTM D2240
Tensile Strength at Break 55.0 MPaDIN 53504
Elongation at Break 590 %ASTM D412
100% Modulus 0.0120 GPa
@Strain 100 %
DIN 53504
300% Modulus 0.0260 GPa
@Strain 300 %
DIN 53504
Rebound 35 %Bayshore; ASTM D2632
Tear Strength 830 pliASTM D624
Abrasion 27[mm3]; ISO 4649
Compression Set 26 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM D395
 46 %
@Temperature 70.0 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 190 - 200 °CHuntsman/TMA
 
Processing PropertiesOriginal ValueComments
Feed Temperature 25.0 - 40.0 °CExtrusion
Front Barrel Temperature 200 - 215 °CExtrusion
Nozzle Temperature 200 - 215 °CExtrusion
Adapter Temperature 200 - 215 °CExtrusion
Die Temperature 200 - 215 °CExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade
Huntsman IROGRAN® A 98 E 4735 Polyester-Based TPU-Injection Extrusion Grade
Huntsman IROGRAN® A 98 H 4661 Polyester-Based TPU-Injection Molding Grade

PHU9921 / 150381

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.