MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Superior Flux Superior No. 430C Organic Acid, Non-Halide Tinning Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Water-based, non-halide organic acid flux.
  • Developed for electronic applications where halide type fluxes are not acceptable.
  • Specially formulated for applications involving Alloy 42, Kovar, Nickel, EN, and Copper.
  • Applications include components, IC's, and semiconductors, cerdips, and connectors.
  • Water-based, non-halide organic acid flux fitting IPC-ANSI-J-Std-004, Type ORH0.
Description: Superior No. 430C is a water-soluble flux that is entirely free of Chlorides, Bromides, and Phosphates. It employs unique organic activators to strip off metal oxides and tarnish, without attacking the underlying metals. This flux has many of the excellent operational characteristics of halide-containing organic fluxes while being much less corrosive.

Applications: COMPONENT TINNING-Superior No. 430C is supplied in concentrated form and provides most effective oxide removal as supplied. The flux may be used as supplied, or diluted, in dip, drag, and other processes common to component tinning. Due to the flux having a low degree of corrosivity, components need not be soldered immediately after fluxing. To remove residues, wash with hot (60°C/ 140°F) distilled or de-ionized water using a non-ionic surfactant.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 - 1.27 g/cc
Density 10.49 lb/gal
pH 2.3 - 2.8
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 280 °CSoldering Range
Shelf Life 2.00 Month
 
Descriptive Properties
ColorClear, straw-colored liquid
ResiduesCompletely water-soluble
Spread Factor>80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSFLUX061 / 185745

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.