MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LATI LASTIROL TR-V0 Polystyrene (PS) (UL94 V-0)  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass fiber reinforced types have high rigidity and excellent dimensional stability.

Specific Notes for this Material: UL94V-0 self-extinguishing, with halogens; heat-resisting version; excellent flowability; good surface finish.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Water Absorption 0.050 %0.050 %at 23°C; ISO 62
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inLATI
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inLATI
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 4545ASTM D785
Tensile Strength, Ultimate 30.0 MPa4350 psiISO 527
 18.0 MPa
@Temperature 60.0 °C
2610 psi
@Temperature 140 °F
ISO 527
Flexural Modulus 2.25 GPa326 ksiASTM D790
 1.90 GPa
@Temperature 60.0 °C
276 ksi
@Temperature 140 °F
ASTM D790
Izod Impact, Notched  0.400 J/cm
@Temperature -40.0 °C
0.749 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 0.500 J/cm
@Temperature -20.0 °C
0.937 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 0.900 J/cm
@Temperature 23.0 °C
1.69 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Charpy Impact Unnotched  3.50 J/cm²
@Temperature -20.0 °C
16.7 ft-lb/in²
@Temperature -4.00 °F
DIN 53453
 3.50 J/cm²
@Temperature -40.0 °C
16.7 ft-lb/in²
@Temperature -40.0 °F
DIN 53453
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 21.0 kV/mm
@Thickness 2.00 mm
533 kV/in
@Thickness 0.0787 in
IEC 243-1
Comparative Tracking Index 250 V250 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C201 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FASTM D648
Vicat Softening Point 94.0 °C201 °F50°C/h 50N; ISO 306
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Glow Wire Test  960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 695-2-1
 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 170 - 190 °C338 - 374 °F
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Drying Temperature 60.0 - 70.0 °C140 - 158 °FTemperature can be reduced when using vacuum ovens.
Dry Time >= 3 hour>= 3 hourDrying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Heat Resistance - Ball Test (125°C)NIEC 335
Heat Resistance - Ball Test (165°C)NIEC 335
Injection Speedmedium
Needle Burner TestY1.47 mm
 Y3.05 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Retain® PS-4578 Polystyrene
Cossa Polimeri ESTASTIR HI 1012 Polystyrene
Cossa Polimeri ESTASTIR HI 10 V0 Flame Retardant Polystyrene
Chi Mei Polyrex® PH-88S Polystyrene - Extrusion
Chi Mei Polyrex® PG-383 Polystyrene

PLATI158 / 50156

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.