Trigonox B-C50 is an initiator (50% active ingredient in isododecane) for (co)polymerization of (meth)acrylates. CAS number: 110-05-4 EINECS/ELINCS No: 203-733-6 Applications: Polymerization of ethyleneTrigonox B-C50 is an efficient initiator for the production of Low Density Polyethylene (LDPE). It is used both for tubular and autoclave processes. In most cases a combination with other peroxides is used to ensure a broad reactivity range. Information provided by Nouryon |