MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Okulen® OKULEN® 1000 – blue – FN5100 UHMW-PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: OKULEN® 1000 is a ultra high molecular low pressure polyethylene with a molecular weight of approx. 5.000.000 g/mol (UHMW-PE)

Properties: Good wear resistance; Very high notched impact strength; Very good sliding properties; Extremely versatile; EU 1935/2004 & 10/2011 – conform; FDA – conform

Color: blue FN5100/similar RAL 5015

Range of applications: Mechanical industry; Conveying industry; Food industry; Chemical industry

Information provided by Okulen

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccDIN EN ISO 11831-1
Water Absorption <= 0.010 %DIN EN ISO 62
Molecular Weight 5.00e+6 g/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61 - 65
@Time 3.00 sec
6 mm plate; DIN EN ISO 868
Ball Indentation Hardness 35.0 MPaDIN EN ISO 2039
Tensile Strength, Yield >= 18.0 MPa1B- 50 mm/min; DIN EN ISO 527-2
Elongation at Break >= 350 %1B- 50 mm/min; DIN EN ISO 527-2
Tensile Modulus >= 650 MPa1B- 1 mm/min; DIN EN ISO 527-2
Izod Impact, Notched (ISO) 140 kJ/m²DIN EN ISO 21304-2
Coefficient of Friction, Dynamic 0.10 - 0.15ASTM D1894
Coefficient of Friction, Static 0.15 - 0.20ASTM D1894
Abrasion 100Sand-Slurry; DIN EN ISO 15527
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmDIN EN 62631-3-1
Surface Resistance >= 1.00e+13 ohmDIN EN 62631-3-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 - 20.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359
Thermal Conductivity 0.410 W/m-K
Melting Point 133 - 135 °CDIN EN ISO 11357-1
Flammability, UL94 HB
 
Descriptive Properties
Operation Temperature80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

POKUL1017 / 307294

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.