System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
DuPont Mobility and Materials Zytel® 79G13HSL BK039 PA66-IGF13
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 10% Glass Fiber Filled
Material Notes:
13% Glass Reinforced, Toughened, Heat Stabilized, Polyamide 66
While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.21
g/cc
DAM; ISO 1183
Linear Mold Shrinkage, Flow
0.0050
cm/cm
DAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse
0.0080
cm/cm
DAM; ISO 294-4, 2577
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
67.0
MPa
50% RH; ISO 527-1/-2
115
MPa
DAM; ISO 527-1/-2
Elongation at Break
4.0 %
DAM; ISO 527-1/-2
10 %
50% RH; ISO 527-1/-2
Tensile Modulus
3700
MPa
50% RH; ISO 527-1/-2
5100
MPa
DAM; ISO 527-1/-2
Poissons Ratio
0.35
DAM; ISO 527-1/-2
0.36
50%RH; ISO 527-1/-2
Izod Impact, Notched (ISO)
7.50
kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
10.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched
54.0
kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
59.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
59.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
67.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched
6.00
kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
6.00
kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
8.00
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
12.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Thermal Properties
Original Value
Comments
Melting Point
262
°C
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
260
°C
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
240
°C
DAM; ISO 75-1/-2
Flammability, UL94
HB
@Thickness 0.800 mm
DAM; IEC 60695-11-10
HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread
24.0
mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Processing Properties
Original Value
Comments
Melt Temperature
295
°C
Injection Optimum
285
-
305
°C
Injection
Mold Temperature
50.0
-
100
°C
Injection
80.0
°C
Injection Optimum
Ejection Temperature
210
°C
Drying Temperature
80.0
°C
Dry Time
2.00
-
4.00
hour
Dehumidified Dryer
Moisture Content
0.20 %
Hold Pressure
50.0
-
100
MPa
Descriptive Properties
Drying Recommended
yes
Emission of organic compounds (µgC/g)
13
VDA 277
FMVSS Class
B
ISO 3795 (FMVSS 302)
Fogging (mg)
0.3
G-value (condensate); ISO 6452; DAM
Hold pressure time (s/mm)
3
Max. screw tangential speed (m/s)
0.2
DAM
Odor
4
VDA 270
Part Marking Code
PA66-IGF13
ISO 11469
Processing
Injection Molding
Regional Availability
Europe
Near East/Africa
Resin Identification
PA66-IGF13
ISO 1043
Special characteristics
Heat stabilized or stable to heat
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Celanese Zytel® 70G13L NC010 PA66-GF13
Celanese Zytel® 70G13HS1L BK031 PA66-GF13
DuPont Mobility and Materials Zytel® 79G13HSL NC010 PA66-IGF13
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Conditioned)
Celanese Zytel® 70G33HS1L BK031 PA66-GF33
PDSX5371 / 198011
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.