MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics CHO-SHRINK® Boots Conductive Heat Shrinkable EMI Shielding
Categories: Polymer; Thermoset

Material Notes: Description: CHO-SHRINK connector boots provide EMI shielding, cable shield grounding, and strain relief at connector backshell terminations. A highly conductive silver-based coating applied to the inside surface of these molded polyolefin boots provides 60-80 dB attenuation above 500 MHz and in combination with braid will provide levels of attenuation exceeding 80 dB above 10 GHz. CHO-SHRINK boots shrink to a wide range of cable diameters (shrink ratio is 4:1 at the cable end), and offer a 40-65% weight savings compared to metal EMI adapters. They can be supplied with a conductive hot melt adhesive/sealant applied to each end. Normal shrink temperatures assure good joining and sealing at boot/connector interfaces. To specify hot-melt option, see table foot-notes. For optimum mechanical strength, CHO-SHRINK lipped boots should be shrunk over shrink boot adapters which provide a knurled and grooved surface. In addition, plastic tie-wraps should be installed over both ends of boot after shrinking. CHO-SHRINK cable transitions, including T, Y and other custom shapes, are also available.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 7.78 kV/mm198 kV/inASTM D876
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Descriptive Properties
Shrink Ratioup to 4:1
Shrink Temperature121 - 191°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME239 / 130949

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.