MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman Propyl Acetate Solvent
Categories: Fluid; Solvent

Material Notes: CAS No. 109-60-4

Product Description: Eastman™ Propyl Acetate is a colorless liquid with a mild, fruity odor. It is an active solvent for nitrocellulose, cellulose acetate butyrate, polyester, alkyd, and acrylic resins. Eastman™ Propyl Acetate has a medium evaporation rate and is a non-HAP solvent. It promotes flow and leveling in a variety of formulations.

Application/Uses:

  • Coatings - Automotive OEM
  • Coatings - Automotive Refinish
  • Coatings - Can and Coil
  • Coatings - General Industrial
  • Coatings - Industrial Maintenance and Marine
  • Coatings - Industrial Wood
  • Coatings - Transportation
  • Cosmetics and Personal Care - Nail Care and Flavoring Agent
  • Graphic Arts - Printing Inks
Key Attributes:
  • Excellent solvent activity
  • Good coupling efficiency
  • High dilution ratio
  • Inert - Food use with limitations
  • Inert - Nonfood use
  • Medium evaporation rate
  • Miscible with water and most organic liquids
  • Non-HAP
  • Non-SARA
  • Readily biodegradable

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.889 g/cc
Viscosity 0.60 cPLiquid
Molecular Weight 102.14 g/mol
Vapor Pressure 0.0303 atm
@Temperature 20.0 °C
 0.186 atm
@Temperature 55.0 °C
Surface Tension 24.3 dynes/cm
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 33.2 atm
Critical Temperature 276.5 °C
Total Acid Number <= 0.010
 
Thermal PropertiesOriginal ValueComments
CTE, linear 126 µm/m-°C
Melting Point -92.0 °CFreezing Point
Boiling Point 99.0 - 103 °C@ 760 mm Hg
Flash Point 13.0 °CTag Closed Cup
 14.0 °CTag Open Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.38
 
Descriptive Properties
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5258 / 222452

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.