MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Techtron® HPV PPS (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Unreinforced, Extruded

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D792
Water Absorption 0.010 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.090 %Immersion; ASTM D570(2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 84ASTM D785
Tensile Strength 10900 psiASTM D638
Tensile Strength at 150°C (300°F) 500 psiASTM D638
Tensile Strength at 65°C (150°F) 8000 psiASTM D638
Elongation at Break 4.0 %ASTM D638
Tensile Modulus 540 ksiASTM D638
Flexural Strength 10500 psiASTM D790
Flexural Modulus 535 ksiASTM D790
Compressive Strength 15500 psi10% Def.; ASTM D695
Compressive Modulus 342000 psiASTM D695
Izod Impact, Notched 1.40 ft-lb/inASTM D256 Type A
Coefficient of Friction, Dynamic 0.20Dry vs. Steel; QTM55007
K (wear) Factor 62.0 x 10-10 in³-min/ft-lb-hrQTM 55010
Limiting Pressure Velocity 8750 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+13 ohmEOS/ESD S11.11
Dielectric Strength 500 V/milShort Term; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Thermal Conductivity 2.10 BTU-in/hr-ft²-°FASTM F433
Melting Point 536 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 430 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 240 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
Estimated Rating
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG No
FDA Yes
NSF No
USDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Conductive / Static Dissipative No
Continuous Sunlight Limited
Hot Water / Steam Acceptable
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Descriptive Properties
Machinability31-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS); Molded
Mitsubishi Chemical Advanced Materials Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Fluorosint® 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers (ASTM Product Data Sheet)

P1SM36 / 20128

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.