MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wellman Expond® C3322T-FNS Polypropylene, 20% Mineral
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Expond® Polypropylene (PP) is a linear polymer with low density and typically exhibits high crystallization. It consistently has relatively high performance characteristics, such as good mechanical equilibrium, chemical corrosion resistance, workability, low price and other advantages.

Features: Excellent balance of toughness and stiffness, Low-odor, low-VOC, and low-emission performance, Excellent scratch resistance performance, Excellent anti-stick performance, Excellent resistance to stress performance Excellent weather fastness performance, Easy to process, Excellent spraying performance.

Applications: Automotive Dashboard, Door, Column, Seat guard plate, Bumper, Rubbing strip, Bottom plate.

Information provided by Wellman Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183-1
Filler Content 20 %Mineral; ISO 3451
Linear Mold Shrinkage 0.010 - 0.012 cm/cmPRET
Melt Flow 22 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 19.0 MPa50mm/min; ISO 527-2
Elongation at Yield 4.7 %50mm/min; ISO 527-2
Flexural Modulus 1500 MPa2mm/min, 40mm; ISO 178
Izod Impact, Notched (ISO) 30.0 kJ/m²ISO 179-1/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 163.3 °CISO 3146
Flame Spread 43.0 mm/minTL 1010
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 200 °CInjection Temperature
 200 - 220 °CInjection Temperature
 210 - 230 °CInjection Temperature
Mold Temperature 20.0 - 60.0 °C
Drying Temperature 80.0 - 90.0 °C
@Time 3600 - 7200 sec
Moisture Content 0.10 %
Injection Pressure 50.0 - 80.0 MPa
Back Pressure 0.300 - 1.00 MPa
Screw Speed 40 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWEL00868 / 249992

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.