MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen PP H2150 304850 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Hostalen PP H2150 304850 is a polypropylene homopolymer, grey colored similar to RAL 7032 (pebble grey) and is typically used in the applications of compression molded filters and sheets. Applications: General Sheet Extrusion, Industrial

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccISO 1183-1
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 0.50 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 1.3 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67ISO 868
Tensile Strength, Yield 36.0 MPaISO 527-1,-2
Elongation at Yield 10 %ISO 527-1,-2
Tensile Modulus 1500 MPaISO 527-1,-2
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -20.0 °C
ISO 179
 5.00 kJ/m²
@Temperature 0.000 °C
ISO 179
 38.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 95.0 °CA50N; ISO 306
 156 °CA50; ISO 306
DSC Induction Temperature 159 °CISO 3146
 
Descriptive Properties
Processing Methodcompression molding, pipe, sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom PP HH42L 356015 Polypropylene
LyondellBasell Hostalen PP H2142 12 Polypropylene Copolymer
LyondellBasell Hostalen PP H1850 Polypropylene Copolymer
LyondellBasell Hostalen PP H1022 Polypropylene Copolymer
LyondellBasell Hostacom TRG 436P NAT Polypropylene, Glass/Mineral Reinforced

PEQT8508 / 220143

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.