MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ravago Petrochemical Ravathane® R130A93 Ester-Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Typical properties: excellent abrasion and scratch resistance, high elasticity, high tensile & tear strength, good oil and grease resistance, low temperature flexibility, recyclable, adhesion to polar substrates. Applications: Shoe soles, tactile markers, castor wheels, hose & tubing, timing belt, animal identification tags.

Information provided by Ravago Petrokimya (Ravago Petrochemical).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 11831-A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393ISO 868
Tensile Strength 40.0 MPa5800 psiISO 37
Elongation at Break 575 %575 %ISO 37
100% Modulus 9.50 MPa
@Strain 100 %
1380 psi
@Strain 100 %
ISO 37
300% Modulus 19.0 MPa
@Strain 300 %
2760 psi
@Strain 300 %
ISO 37
Izod Impact, Notched (ISO)  35.0 kJ/m²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
Izod Impact, Unnotched (ISO)  55.0 kJ/m²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
Tear Strength 165 kN/m941 pliISO 34-1/B/b
Abrasion 4040mm3; ISO 4649
Compression Set  20 %
@Temperature 23.0 °C,
Time 79200 sec
20 %
@Temperature 73.4 °F,
Time 22.0 hour
ISO 815-1
 40 %
@Temperature -30.0 °C,
Time 79200 sec
40 %
@Temperature -22.0 °F,
Time 22.0 hour
ISO 815-1
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F
Vicat Softening Point 125 °C257 °FISO 306-A
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 195 - 215 °C383 - 419 °F
Moisture Content <= 0.10 %<= 0.10 %Drying is important

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 2420F Low Density Polyethylene (LDPE), Blown Film Grade
EMS-Grivory Grilamid® TR 90 PAMACM12
EMS-Grivory Grilamid® TR 90 NZZ nat PAMACM12-I
C.O.I.M. LARIPUR® LPR9025 Special Adipate Ester Polyurethane
Ravago Petrochemical Ravathane® R130A70 Ester-Based Thermoplastic Polyurethane

PRAVAGO910 / 198200

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.