MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Novec™ Contact Cleaner/Lubricant
Categories: Fluid

Material Notes: 3M™ Novec™ Contact Cleaner/Lubricant penetrates and flushes away light oils and greases from electrical and electronic equipment. Removes fluorinated oils and grease, leaving a thin protective silicone coating. Meets MIL-PRF 29608A Class L specs.

Features and Benefits:

  • Cleans and lubricates
  • Non-flammable
  • Excellent plastics compatibility
  • Non-conductive, non-corrosive
  • Meets MIL PRF 29608A Class L
  • Low toxicity
  • Low Global Warming Potential
  • Contains No HCFCs, HFCs, nPB or HAPs

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³
Surface Tension 15.3 dynes/cm15.3 dynes/cm
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 0.984 kV/mm>= 25.0 kV/in
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Novec™ 7100DL Engineered Fluid
3M Novec™ 7100 Engineered Fluid
3M Novec™ 7000 Engineered Fluid
3M Novec™ 649 Engineered Fluid
3M Novec™ 71DA Engineered Fluid

PMM33123 / 167870

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.