MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Wacker Cavamax® W7 FOOD Beta-cyclodextrin
Categories: Other Engineering Material

Material Notes: CAVAMAX® W7 Food is food grade beta-cyclodextrin. CAVAMAX® W7 Food with 7 glucose units has the mid-sized cavity of the parent cyclodextrins. It is useful as a flavor protectant in Human food.

Empirical formula: C42H70O35

CAS No.: 7585-39-9

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.400 - 0.700 g/cc0.0145 - 0.0253 lb/in³
Molecular Weight 1135 g/mol1135 g/mol
Ash <= 0.1 %<= 0.1 %sulfate ash
Evaporation Loss <= 14 %<= 14 %
 
Descriptive Properties
Appearancesolid -powder
Colorwhite
Content<0.5%Reducing substances (determined as dextrose)
 <1 ppmLead
 <1 ppmVolatile organics
 <1.3 ppmArsenic
 <1000 CFU/gMicroorganisms
 <5 ppmHeavy metals
 >98%Content (on dry basis)
 0 in 10 gSalmonella/E Coli
Solubility18.5 g/lOECD 105, in water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9051 / 204580

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.