NAV128 Y40-03 is a transparent dark polypropylene (PP) post-industrial recycled supplied in pellets. This product is an ideal PP used where sustainability and circularity matter. NAV128 Y40-03 consists of post-industrial waste coming from Borealis plants. Due to the nature of recycleds, some variation in color can be observed between batches. Typical characteristics: - Good stiffness / impact balance
- Low odor
- Good demolding properties
- Available in homogenized 12-ton batches
Applications:- Injection molding applications
Information provided by Borealis AG |