MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled; Polyethylene Terephthalate (PET)

Material Notes: Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handles, toaster casings, external mirrors, rear screen wiper arms in vehicles and sunroof wind deflectors.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 - 0.900 g/cc
Density 1.73 g/ccISO 1183
Water Absorption 0.40 %ISO 62
Moisture Absorption at Equilibrium 0.20 %ISO 62
Viscosity Test 90 cm³/gISO 307
Linear Mold Shrinkage, Flow 0.0010 cm/cmplate with film gate 150x150x3mm3
 0.0024 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.0075 cm/cmplate with film gate 150x150x3mm3
 0.0077 cm/cmISO 2577
Melt Flow 67.47 g/10 min
@Load 10.0 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 165 MPa50 mm/min; ISO 527-1/-2
Elongation at Break 1.5 %ISO 527-1/-2
Tensile Modulus 18700 MPaISO 527-1/-2
Charpy Impact Unnotched 52.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 58.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Dielectric Constant 4.5
@Frequency 1e+6 Hz
IEC 60250
 4.7
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0020
@Frequency 100 Hz
IEC 60250
 0.015
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 225 VTest Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-1/-2
Melting Point 235 °CISO 11357-1/-2
Maximum Service Temperature, Air 140 °Cat 50% loss of tensile strength after 20,000hr
 160 °Cat 50% loss of tensile strength after 5,000hr
 210 °C
Deflection Temperature at 0.46 MPa (66 psi) 221 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75-1/-2
Decomposition Temperature >= 290 °C
Flammability, UL94 HB
@Thickness >=0.400 mm
 HB
@Thickness 1.60 mm
Ignition Temperature 350 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °CHopper Throat
Zone 1 260 °CFeed zone
Zone 2 265 °CCompression
Zone 3 270 °CMetering-zone
Zone 4 270 °CNozzle
Melt Temperature 250 - 280 °CInjection molding/Extrusion
 270 °COptimal
Mold Temperature 60.0 - 100 °CInjection molding
 80.0 °COptimal
Drying Temperature 80.0 - 120 °C
Dry Time 4 hour
Moisture Content <= 0.040 %
 
Descriptive Properties
ColorBK 15029
Commercial StatusEurope
Peripheral Screw Speed< 0.25 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET
BASF Petra® 7010 WT 7729 15% Glass Filled PET
BASF Ultradur® B 4040 G6 30% Glass Filled PBT + PET
BASF Petra® 7010 BK 5830 15% Glass Filled PET

PBASG0123 / 131756

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.