MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Applied Silicone 40024 Liquid Silicone Rubber, 20 Durometer (LSR 20), Implant Grade
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Injection Molding

Information provided by Applied Silicone Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2020Typical
 16 - 2516 - 25
Tensile Strength >= 5.17 MPa>= 750 psi
 5.52 MPa800 psiTypical
Elongation at Break >= 550 %>= 550 %
 660 %660 %Typical
200% Modulus 0.862 MPa
@Strain 200 %
125 psi
@Strain 200 %
Tear Strength >= 17.5 kN/m>= 100 pli
 21.0 kN/m120 pliTypical
 
Processing PropertiesMetricEnglishComments
Extrusion Rate 220 g/min220 g/minTypical
Cure Time 5.00 min
@Temperature 175 °C
0.0833 hour
@Temperature 347 °F
 
Descriptive Properties
Cure SystemPlatinum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NuSil MED2-6600 Elastomeric Dispersion Biomedical Elastomer
Mearthane Durethane™ S DS-720A Solid Polyurethane Elastomer
ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer
Elkem (Bluestar Silicones) SILBIONE® LSR 4305 Liquid Silicone Rubber
Dow Silastic® P-1 RTV SILICONE RUBBER & BLUE CURING AGENT

PNUSILA902 / 194571

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.